Various casting defects in a ~13" diameter ASTM A990 Grade CN3MCu (Modified) cast impeller • Royalty Free Stock Photo
Royalty Free Stock Image from Shutterstock 1430413178 by lbrumf2
Shutterstock ID | 1430413178 |
---|---|
Added | June 21, 2019 (5 years ago) |
Ratio | 1.5 |
Adult | NO |
Med size (JPG) | 1000 x 667 px, 0.9 Mb, 300 DPI |
Small size (JPG) | 500 x 334 px, 0.2 Mb, 300 DPI |
Huge size (JPG) | 3504 x 2336 px, 7.5 Mb, 300 DPI |
Download Free Images
More than 400 000 free photos available for download
Various casting defects in a ~13" diameter ASTM A990 Grade
CN3MCu (Modified) cast impeller is royalty free stock photo by lbrumf2.